ERNiCrMo-8

Class: ERNiCrMo-8
AWS: A5.14

Conforms to Certification: AWS A5.14 | ASME SFA A5.14

Weld Process: GTAW Welding Processes

AWS Chemical Composition Requirements
C = 0.03 max Cu = 0.7 – 1.2
Mn = 1.0 max Ni = 47.0 – 52.0
Fe = Remainder Ti = 0.7 – 1.5
P = 0.03 max Cr = 23.0 – 26.0
S = 0.03 max Mo = 5.0 – 7.0
Si = 1.0 max Other = 0.50 max

Please Call For More Information and Available Sizes

Application
ERNiCrMo-8 is used for welding nickel-chromium-molybdenum base materials to itself, steel and other nickel base alloys, and for cladding steel with NI-CR-MO weld materials.

Deposited Chemical Composition % (Typical)
C = 0.01 Cr = 24.75 Ni = 50.5
Cu = 0.90 Mo = 6.1 Fe = Balance
Si = 0.70
Deposited All Weld Metal Properties % (AW) 
Tensile Strength 91,000 psi
Elongation 27%

Deposited Charpy-V-Notch Impact Properties %
Not applicable

Recommended Welding Parameters for TIG, MIG, and SAW Welding of Nickel Alloys

Process Diameter of Wire Voltage (V) Amperage (A) Gas
Tig .035 inches x 36 12 – 15 60 – 90 100% Argon
.045 inches x 36 13 – 16 80 – 110 100% Argon
1/16 inches x 36 14 – 18 90 – 130 100% Argon
3/32 inches x 36 15 – 20 120 – 175 100% Argon
1/8 inches x 36 15 – 20 150 – 220 100% Argon

Note:  Other shielding Gases may be used for Tig welding. Shielding gases are chosen taking Quality, cost, and Operability into consideration.

Note:  Both agglomerated and fused fluxes can be used for submerged arc welding.

Note: The chemical composition of the flux mainly affects the chemistry of the weld metal and consequently its corrosion resistance and mechanical properties.