ER90S-B9

Class: ER90S-B9
AWS: A5.28

Conforms to Certification: AWS A5.28 | ASME SFA A5.28

Weld Process: Tig (GTAW) Welding Processes

AWS Chemical Composition Requirements
C = 0.07 – 0.13 Mn = 1.20 max
Si = 0.15 – 0.50 P = 0.010 max
S = 0.010 max Ni = 0.80 max
Cr = 8.00 – 10.50 Mo = 0.85 – 1.20
V = 0.15 – 0.30 Al = 0.04 max
Cu = 0.20 max N = 0.03 – 0.07
Nb = 0.02 – 0.10 Other = 0.50 max
 Note:  the sum of Mn + Ni shall be less than or equal to 1.50% max.

Available Sizes
.030 x 36
.035 x 36
.045 x 36
1/16 x 36
3/32 x 36
1/8 x 36
3/16 x 36
5/32 x 36

Application
Material contains 9% chromium and 1% molybdenum. Classification is intended for welding base materials of similar composition. Requires controlled preheat, inter-pass and post-weld heat treatment.

Deposited Chemical Composition % (Typical)
C = 0.09 P = 0.009 Cr = 8.75
Mn = 0.85 S = 0.009 Mo = 1.08
Si = 0.20 Ni = 0.55 Cu = 0.11
V = 0.19 Nb = 0.08 N = 0.04
Deposited Mechanical Properties (SR) 1400º F for (2) Hours
Tensile Strength 112,000 psi
Yield Strength 100,000 psi
Elongation 17%

Deposited Charpy-V-Notch Impact Properties %
Not Applicable

Available Sizes & Recommended Welding Parameters

Process Diameter of Wire Voltage (V) Amperage (A) Gas
Tig .035 inches x 36 10 – 12 50 – 70 100% Argon
.045 inches x 36 10 – 12 70 – 100 100% Argon
1/16 inches x 36 12 – 15 100 – 125 100% Argon
3/32 inches x 36 15 – 20 125 – 175 100% Argon
1/8 inches x 36 15 – 20 175 – 250 100% Argon