ER308H
Class: ER308H
AWS: A5.9
Conforms to Certification: AWS A5.9 | ASME SFA A5.9
Weld Process Used for Tig: (GTAW)
AWS Chemical Composition Requirements
C = 0.04 – 0.08
Cr = 19.5 – 22.0
Ni = 9.0 – 11.0
Mo = 0.50 max
Mn = 1.0 – 2.5
Si = 0.30 – 0.65
P = 0.03 max
S = 0.03 max
Cu = 0.75 max
Available Sizes
.030 x 36
.035 x 36
.045 x 36
1/16 x 36
3/32 x 36
1/8 x 36
3/16 x 36
5/32 x 36
Application
WW308H is used to TIG welding of un-stabilized stainless steels such as Types 301, 302, 304, 305, 308.
Deposited Chemical Composition % (Typical) | ||
C = 0.04 | Si = 0.32 | Mn = 1.8 |
P = 0.009 | S = 0.009 | Cr = 20.0 |
Ni = 9.5 | N = 0.05 |
Mechanical Properties (R.T.) | |
Yield Strength | 61,000 psi |
Tensile Strength | 90,000 psi |
Elongation | 41% |
Reduction of Area | 60% |
Deposited All Weld Metal Properties
Data is typical for ER308H weld metal deposited by Tig using 100% Argon as the shielding gas.
Recommended Welding Parameters |
|||
GTAW “Tig Process” | |||
Wire Diameter | Amps DCSP | Volts | Shielding Gas |
.035 | 60-90 | 12-15 | Argon 100% |
.045 | 80-110 | 13-16 | Argon 100% |
1/16 | 90-130 | 14-16 | Argon 100% |
3/32 | 120-175 | 15-20 | Argon 100% |
Note: Parameters for tig welding are dependent upon plate thickness and welding position.
Other shielding Gases may be used for Tig welding. Shielding gases are chosen taking Quality, Cost, and Operability into consideration.