ENiCrMo-10 DMNA122
Class: ENiCrMo-10
AWS: A5.11
DURAMAX NA122
Conforms to Certification: AWS A5.11 | ASME SFA 5.11
Weld Process: Shielded Metal Arc Weld Process (SMAW)
AWS Chemical Composition Requirements | |
C = 0.02 max | Cu = 0.50 max |
Mn = 1.0 max | Ni = Remainder |
Fe = 2.0 – 6.0 | Co = 2.5 max |
P = 0.03 max | Cr = 20.0 – 22.5 |
S = 0.015 max | Mo = 12.5 – 14.5 |
Si = 0.20 max | W = 2.5 – 3.5 |
V = 0.35 max | Other = 0.50 max |
Please contact us for more information and availability
Application
DURAMAX NA122 (ENiCrMo-10) has a nominal composition (wt.-%) of 56 Ni, 22 Cr, 13 Mo, 4 Fe, 3W. Electrodes of this classification are used for welding nickel chromium-molybdenum alloys, for the welding of the clad side of joints in steel clad with nickel-chromium-molybdenum alloy, to steel and to other nickel-base alloys; and for joining nickel-chromium-molybdenum alloys. Typical specifications for the nickel-chromium-molybdenum base metals are ASTM B 574, B 575, B 619, B 622, and B 626, all of which have UNS Number N06022.
DMNA122 is formulated for welding a wide array of industrial applications including power generation, petroleum and chemical plants, as well as offshore and marine facilities.
Deposited Chemical Composition % (Typical) | ||
C = 0.012 | Mn = 0.16 | Fe = 2.24 |
P = 0.003 | S = 0.001 | Si = 0.19 |
Cu = 0.05 | Ni = 57.34 | Co = 0.01 |
Cr = 22.14 | Mo = 14.22 | V = 0.03 |
W = 3.45 | TOE = <0.50 |
Deposited All Weld Metal Properties % (AW) | |
Tensile Strength | 720 N/mm2 |
Yield Strength | 538 N/mm2 |
Elongation | 38% |
Deposited Charpy-V-Notch Impact Properties %
Not applicable
Recommended Weld Parameters |
Amperage (A) |
||
Diameter of Wire | Voltage (V) | Flat | Vertical and Overhead |
3/32 inches (2.4mm) | 20 – 23 | 70 – 80 | 65 – 80 |
1/8 inches (3.2mm) | 21 – 24 | 80 – 110 | 75 – 95 |
5/32 inches (4.0mm) | 22 – 25 | 120 – 160 | Not recommended |
3/16 inches (4.8mm) | 23 – 25 | 170 – 190 | Not recommended |