ERNiCrMo-9
Class: ERNiCrMo-9
AWS: A5.14
Conforms to Certification: AWS A5.14 | ASME SFA A5.14
Weld Process: GTAW Welding Process
AWS Chemical Composition Requirements | |
C = 0.015 max | Cu = 1.5 – 2.5 |
Mn = 1.0 max | Ni = Remainder |
Fe = 18.0 – 21.0 | Co = 5.0 max |
P = 0.04 max | Cr = 21.0 – 23.5 |
S = 0.03 max | Nb + Ta = 0.50 max |
Si = 1.0 max | Mo = 6.0 – 8.0 |
W = 1.5 max | Other = 0.50 max |
Please Call For More Information and Available Sizes
Application
ERNiCrMo-9 is used for welding nickel-chromium-molybdenum base materials to themselves, steel and other nickel base alloys, and for cladding steels.
Deposited Chemical Composition % (Typical) | ||
C = 0.01 | Cr = 22.0 | Ni = Balance |
Cu = 2.0 | Mo = 7.1 | Fe = 20.5 |
Co = 2.75 |
Deposited All Weld Metal Properties % (AW) | |
Tensile Strength | 96,000 psi |
Elongation | 29% |
Deposited Charpy-V-Notch Impact Properties %
Not applicable
Recommended Welding Parameters for TIG, MIG, and SAW Welding of Nickel Alloys |
||||
Process | Diameter of Wire | Voltage (V) | Amperage (A) | Gas |
Tig | .035 inches x 36 | 12 – 15 | 60 – 90 | 100% Argon |
.045 inches x 36 | 13 – 16 | 80 – 110 | 100% Argon | |
1/16 inches x 36 | 14 – 18 | 90 – 130 | 100% Argon | |
3/32 inches x 36 | 15 – 20 | 120 – 175 | 100% Argon | |
1/8 inches x 36 | 15 – 20 | 150 – 220 | 100% Argon |
Note: Other shielding Gases may be used for Tig welding. Shielding gases are chosen taking Quality, cost, and Operability into consideration.
Note: Both agglomerated and fused fluxes can be used for submerged arc welding.
Note: The chemical composition of the flux mainly affects the chemistry of the weld metal and consequently its corrosion resistance and mechanical properties.