ERNiCu-7
Class: ERNiCu-7
AWS: A5.14
Conforms to Certification: AWS A5.14 | ASME SFA A5.14
Weld Process: GTAW Welding Process
AWS Chemical Composition Requirements | |
C = 0.15 max | Cu = Remainder |
Mn = 4.0 max | Ni = 62.0 – 69.0 |
Fe = 2.5 max | Al = 1.25 max |
P = 0.02 max | Ti = 1.5 – 3.0 |
S = 0.015 max | Other = 0.50 max |
Si = 1.25 max |
Available Sizes
.035 x 36
.045 x 36
1/16 x 36
3/32 x 36
1/8 x 36
Application
ERNiCu-7 (NA60) is a copper-nickel alloy base wire for GMAW and GTAW welding of Monel alloys 400 and 404. Also used for overlaying steel after first applying Layer of 610 nickel.
Deposited Chemical Composition % (Typical) | ||
C = 0.05 | P = 0.008 | Ni = 65.9 |
Mn = 3.45 | S = 0.002 | Ti = 2.25 |
Fe = 0.40 | Si = 0.77 | Al = 0.10 |
Cu = Balance |
Deposited All Weld Metal Properties % (AW) | |
Tensile Strength | 76,000 psi |
Yield Strength | 51,000 psi |
Elongation | 34% |
Deposited Charpy-V-Notch Impact Properties %
Not applicable
Recommended Welding Parameters for TIG, MIG, and SAW Welding of Nickel Alloys |
||||
Process | Diameter of Wire | Voltage (V) | Amperage (A) | Gas |
Tig | .035 inches x 36 | 12 – 15 | 60 – 90 | 100% Argon |
.045 inches x 36 | 13 – 16 | 80 – 110 | 100% Argon | |
1/16 inches x 36 | 14 – 18 | 90 – 130 | 100% Argon | |
3/32 inches x 36 | 15 – 20 | 120 – 175 | 100% Argon | |
1/8 inches x 36 | 15 – 20 | 150 – 220 | 100% Argon |
Note: Other shielding Gases may be used for Tig welding. Shielding gases are chosen taking Quality, cost, and Operability into consideration.
Note: Both agglomerated and fused fluxes can be used for submerged arc welding.
Note: The chemical composition of the flux mainly affects the chemistry of the weld metal and consequently its corrosion resistance and mechanical properties.